- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Fagor Arrasate participates in development of smart shears for high-strength steel
- September 2, 2020
- News Release
- Shearing
Fagor Arrasate, a designer and manufacturer of presses, coil cutting and processing lines, and systems for manufacturing complex metal parts, is participating in a European investigation project to design smart shears for high-strength steel with a predictive system that warns about cutting tool deterioration.
The project, called IntellCutProcess, will analyze the various parameters that are involved during the cutting process, such as cutting strength, the die looseness or separation, and the cutting angle. The data obtained will allow for the optimization of the cutting tool regarding aspects such as the material used and the protective coating.
The shear will be equipped with sensors that will measure the different cutting quality indicators, such as the burr height and the cutting area profile. With this information, the system will be able to monitor the cutting tool's degradation state. In addition, the predictive system will allow for scheduled production downtime for required interventions.
To validate the results of the research, a fully sensorized shear prototype for the cutting of heavy-thickness metal sheet will be built first. Afterward the new equipment will be installed in an actual operational cutting line.
The program is financed by the European Union’s RFCS-2019 (Research Fund for Coal and Steel) Program, in which six partners participate.
Related Companies
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/07/2024
- Running Time:
- 67:38
Patrick Brunken, VP of Addison Machine Engineering, joins The Fabricator Podcast to talk about the tube and pipe...
- Trending Articles
How laser and TIG welding coexist in the modern job shop
Young fabricators ready to step forward at family shop
Material handling automation moves forward at MODEX
A deep dive into a bleeding-edge automation strategy in metal fabrication
BZI opens Iron Depot store in Utah
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,