- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Shape Corp. roll forms martensitic steel bumper made with fossil-free steel
- June 8, 2023
- News Release
- Roll Forming
Shape Corp., a Grand Haven, Mich.-based global Tier 1 supplier, has manufactured a roll formed, production-intent martensitic steel bumper made with fossil-free steel from SSAB. This material is produced using HYBRIT technology, which replaces coal with hydrogen in the reduction process, powered by fossil-free electricity.
Shape reports it is the first automotive company to collaborate with SSAB in using this sustainable material in the development of this type of automotive component. SSAB aims to produce the steel at a commercial scale in 2026.
Shape has conducted rigorous testing, including bendability, fracture characterization, material toughness, delayed fracture testing, and welding evaluations that have shown the fossil-free steel does not compromise material properties or performance.
The roll forming process not only enables the usage of the highest-strength materials but also promotes efficient section design to optimize the usage of the material, all leading to sustainable manufacturing.
"Our material characterization activity ensures that the performance of this fossil-free steel matches that of the incumbent steelmaking process,” said Brian Oxley, project manager at Shape Corp. “Considering the full scope of emissions in the steelmaking and part production processes, we calculate a savings of over 10.74 kg CO2 (85.7%) for each bumper beam produced with this steel compared to a part made from conventional steel. Those savings can be closer to 20 kg per part when compared to a stamped bumper of similar performance. Those savings will continue to increase as emissions from both processes are reduced further."
Related Companies
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/07/2024
- Running Time:
- 67:38
Patrick Brunken, VP of Addison Machine Engineering, joins The Fabricator Podcast to talk about the tube and pipe...
- Trending Articles
Young fabricators ready to step forward at family shop
Material handling automation moves forward at MODEX
A deep dive into a bleeding-edge automation strategy in metal fabrication
White House considers China tariff increases on materials
BZI opens Iron Depot store in Utah
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,