Contributing Writer
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Tips for tackling virtual sharp points and bend lines for oblique angles
Alternative ways of documenting sheet metal characteristics can lead to more easy-to-understand CAD drawings
- By Gerald Davis
- December 29, 2023
- Article
- Manufacturing Software
When it comes to 3D modeling, a CAD jockey usually has more than one way to solve a design puzzle in CAD.
For example, the creation of a virtual sharp point located at the intersection of two lines is easy if you know how. In another example, bend lines on a sheet metal drawing can be addressed with a bit of manual intervention.
Virtual Sharps and the Z Dimension
Figure 1A presents a sheet metal bracket as it is being edited/reviewed in mainstream 3D CAD. A miter-flange feature (commonly referred to as a 45-degree jog bend) is selected for review, and its dimensioned three-line sketch is (barely) visible in this isometric view.
The CAD sheet metal software converts the simple 2D sketch into a perfect 3D representation of a jogged bend. The miter-flange feature results in easy editing control over angles, inside bend radii, thickness, and dimensions.
Perfect isn’t the same as realistic, but it is suitable and desirable for flat layouts and fabrication planning. 3D CAD does not (easily) model the tooling mars or dents from tooling pressure, but it does model jog bends that resemble reality and are easy to CAD-edit.
Figure 1B shows part of a 2D drawing—a section view of our sheet metal part. Of note here is the dimension Z 0.818, running along the hypotenuse of the angled bend. The Z dimension in this section view is spanning between the outside virtual sharps of the jog bend.
Sheet metal mechanics are likely to be impressed with outside virtual sharps. The rest of the world likely wonders how to physically inspect dimensions between imaginary points. These are not to be measured, however. The Z may instead be used for a particular method of flat layout calculation.
This method of using intersections (imaginary points) sometimes appears on an in-house shop/tooling drawing. Included in Figure 1B is a CAD tip about how to create the virtual sharps:
- Start with the menu of sketch tools visible.
- While holding the CTRL button, select two lines that intersect.
- Then click to insert a sketch point, which will create an intersection (virtual sharp) that can be used as an anchor for dimensions.
Layering the Bend Line Rules
Figure 2A brings attention to the source of Section B-B shown in Figure 1B—a projected view of the entire part. We note that this projected view has both solid lines and dashed lines to represent features of the sheet metal part.
In the sheet metal trade, a dashed line means you are looking at the outside of the bend, and a solid line means you are seeing the inside of the bend. The CAD software complies with these drafting rules and adds dashed or solid lines accordingly.
The CAD software presents the model according to preferences set for the view (such as shaded and wireframe). Two view-preferences affect meaningful dashed lines; Hidden Lines Visible must be selected, and the same for Tangent Edges Removed.
That pair of settings results in automatic bend line generation that complies with drafting standards for 90-degree bends. In other words, those settings properly indicate bend direction.
For bend angles other than 90 degrees, the automatic production of bend lines is somewhat over-helpful, sometimes absent. We note in Figure 2A that, even though the 90-degree bend lines are perfect, the bend lines for the jog bend are invisible. Missing lines are missing compliance with drafting standards.
Figure 2B is an effort to correct the missing line problem from Figure 2A. The view preference for tangent edges has been changed from removed to visible. Now the software is willing to show dashed lines, along with the solid lines not only for bend edges but also for tangent edges. The software feels that the visible tangent edges are necessary to properly interpret the meaning of the dashed bend lines.
With tangent edges visible as extra solid lines, the 90-degree bends are shown with extra solid lines, so we need to understand their meaning (tangent edge, not model edge) in the drawing.
A workaround is to eschew tangent edges and instead use brute force to sketch ideal bend lines for nonperpendicular bends. This brute force is made less brutish by using the Convert Entities tool in combination with automatically generated line entities to sketch without sketching, as it were.
Just make copies of the automatically displayed bend lines (when tangent edges are visible). Such sketched entities will remain visible when the automatic tangent edges are not visible. A brutish result is seen in Figure 2C.
In Figure 2C, the 90-degree automatic bend lines comply with drafting standards, as do the sketched lines for the angled bends. Because our sketched lines are clones of the autogenerated lines, if the bend angle changes, our sketched lines automatically update to maintain proper projection in the drawing’s view.
Here’s a related CAD tip: Layers control how lines are displayed. For examples used in this column, we created and used layers in the drawing. Here’s what was done:
- Dimensions exist in a layer (named DIM) that displays all things with blue ink. That’s a nonstandard preference of the author that helps distinguish dimensions from the model.
- All other layers use black ink.
- A layer (named HID) displays its lines as dashed lines.
Here’s one more CAD tip: To change converted (sketched clone) bend lines from solid lines to dashed lines, CTRL-select all solid miscreants and put them in a layer that displays them as dashed.
Hiding Hidden Clutter
In Figure 3A, a slightly different drafting puzzle is presented. This projected view of the part presents the face with a rectangular cutout along with four related holes. The hidden lines are correct, but cluttering.
In Figure 3B, the preference to hide hidden lines is turned on. That reduces the clutter, but also hides the 90-degree dashed bend lines.
Figure 3C shows the result of cloning the dashed lines and stuffing those clones in the HID layer. Then the hidden lines can be made invisible while the sketched lines remain on display. The view is less cluttered, ready for further detailing.
About the Author
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
What software automation means for custom fabrication
Why employee-owned companies make sense in manufacturing
Nucor’s weekly steel price announcement continues to rattle markets
Press brakes, panel benders, and flat blank calculations
Washington artist creates life-size elk sculptures
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,