Contributing Editor
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Canadian fab shop adds new hydraulic press technology to compete
Backed by 150 years of expertise, Conrex Steel expands capabilities to form thicker material and produce larger tank heads
- By Lindsay Luminoso
- January 23, 2023
- Article
- Bending and Forming
Editor’s Note: This feature originally appeared in the October 2022 issue of Canadian Fabricating & Welding.
Conrex Steel has a long history of serving the tank head and heat-treating industries. Today, the company has over 100,000 sq. ft. of production space across two locations in Toronto and Kingston, Ont., each with their own unique story of longevity and transformation.
A History of Changing Hands
The Toronto location originally was launched in 1948 under the National Welding brand. It was founded as a manufacturer of heads for tank cars and diesel tanks. In 1964, the shop was purchased by Lukens Steel, a U.S. company dating back to 1818. For almost 40 years, the company existed under the name Canadian Lukens Steel until it was purchased by Falvo Steel in 1993, when its name changed to Conrex Steel.
One year later, Conrex was purchased by its current owner Canerector Inc., and has remained one of its legacy acquisitions. Last year, Aberfoyle Metal Treaters and Teffline Coatings became part of the Conrex Group.
“Part of the reason why Lukens Steel purchased National Welding was because of the duties associated with cross-border shipments, so the company saw the need for a Canadian presence,” said Larry Harrison, president,
Conrex Steel Ltd. “They expanded our Canadian operation and invested in different machinery and products. Since we were bought by Canerector, we’ve really honed in on three or four different products including conventional heads, multipiece heads, spheres, and some special forming and custom work.”
The Kingston shop originally was called McKelvey & Birch and founded in 1898. However, it wasn’t until the onset of the World War II that this shop really established itself by providing deep drawing for heavy artillery. After the war, the shop branched out and became C.E. Macpherson, which focused on pipe manufacturing with rolling capabilities and eventually led to the production of dished heads.
Conrex Steel eventually purchased the shop and renamed it Conrex Kingston and focused efforts on conventional hot and cold form dished heads in sizes up to 84 in.
Finding a Way to Stand Out
Conrex has around 50 employees across its operations. Between the two shops, it has 20 tons of trains and a transfer cart system, one of a kind in North America, that acts like an electric 4x4 carrying up to 120,000 lbs. It is used to carry dies and thick material through the shop and into the yard. The Toronto shop sits on 8 acres while Kingston has 5 acres.
Harrison estimates that there are approximately 36 tank head manufacturers in North America. While Conrex has a long history in the industry, Harrison wanted to see how the shop could set itself apart from its competition.
“When I started at the company four years ago, I needed to answer the question ‘What is our competitive advantage?’” he said. “I spent the first couple of months visiting all of our top customers in North America. When I came back, I was able to sort out three things that our customers identified with Conrex: excellent lead times, quality, and customer service. After really understanding our strengths, I wanted to focus on maintaining the strengths while pushing our limits. And because of this, and significant investment in the last couple of years, I believe that we are among the top companies within our industry.”
One of the ways that Harrison tried to set Conrex apart was pushing it towards becoming a one-stop shop. In the last two years, the shop focused on expanding capabilities based on customer feedback.
“I would always ask our customers, ‘What else can we do for you?’” said Harrison. “Feedback included adding elbow forming; pressing thicker, bigger circles; and cutting holes. I took these notes and conferred with the engineering team to find out what we needed to do to deliver.”
Customer feedback helped the shop focus on upgrading various aspects of the tank head manufacturing process.
“We perform robotic cutting, which makes beveling very precise, which is something unique,” said Harrison. “And because of our upgraded robotics, we are able to cut holes in the heads. This was something that no one else seemed to be offering. Almost any head we manufactured would eventually require someone to cut a hole in it as an access point for whatever they were using it for. Because these heads are used for pressure vessels, it’s not that easy to do, especially if the head is not already set up. Some customers were forced to do it manually and work in confined spaces. Adding this capability has been well received.”
The shop presses everything from military-grade HY100, clad materials, stainless steel, and carbon steel. It can form from 3/8- to 6-in.-thick material. To get into some of the thicker materials and bigger heads, the shop installed a new 3,500-ton hydraulic press from Macrodyne Hydraulic Presses in November 2021, the biggest head press in North America, according to Harrison. This new press can process heads that are 1.5 to 7 in. thick with internal dimensions as much as 196 in.
“We are constantly building dies to solve our customers’ challenges and use this press as much as possible,” said Harrison. “We also put in a joggling machine in Kingston to create an offset so that heads can fit into a shell; it crimps the outside part of the head making welding more efficient.”
Tank Head Manufacturing
Conrex focuses on manufacturing different types of tank heads. The most conventional head is a single-piece head that leaves the shop in one piece. Segmental heads are multipiece heads that are often too large to be shipped in one piece. The head segments are formed, fit up, and tack welded. Once they are assembled, they are inspected, the tack weld is removed, and they are shipped in pieces. Conrex has also had a long history producing spheres specifically for the oil and gas fields.
“We really wanted to bring spheres back into play,” said Harrison. “At one point in our history, we were one of the two largest sphere formers in North America. However, when the sphere design changed from the classic orange peel design, we set our sights on once again becoming leaders in this arena.”
The orange peel design required field welding, which was very expensive, oftentimes costing five times what it would to weld in the shop. This led to customers wanting fewer pieces requiring less field welding. The soccer ball design offered that.
“We had to modify our equipment in the shop, reconfigure presses and gantry cranes, so that now we can make the soccer ball sphere,” said Harrison. “What that does is two things. It creates a new revenue stream for us and adds longer-term business.”
Standard heads take anywhere from six to eight weeks to manufacture. Multipiece heads can take up to 12 weeks. However, spheres can take upwards of six months to produce.
“If there is a dip in the economy and we have a good mix of that type of revenue, we won't feel it as much as some shops, where they're all in one segment and have to lay off people,” said Harrison.
Conrex also is focused on taking care of existing equipment, ensuring machine longevity. Right now, the shop is putting in a new CNC table, which Harrison said is essential to the shop’s growth, especially as he believes that companies that fail to upgrade and invest in new technologies could find themselves becoming dinosaurs in the marketplace, and eventually obsolete.
The shop recently has taken on a number of unique projects. For example, it completed a sphere for the underside of a submersible that performs readings from the ocean floor. It’s a thinner sphere than what the shop has ever manufactured before.
“Being thinner meant that it was hard to fit-up, especially because it had such large pieces,” said Harrison. “We needed a lot of support to assemble and tack weld it to ensure that it met all specifications. Same with the soccer-ball-type caps we are making with our new robotics. We had to work through the process but the whole shop was really excited about it. It was unique and that makes it fun. We even manufactured a 6-ft.-wide elbow that we could walk through. It was an engineering feat, but again the challenge made it exciting. We love stuff like this.”
Conrex has some exciting projects on the horizon including one that Harrison was tight-lipped about, only saying that it involves artificial intelligence and that this was an opportunity to expand into a new market.
“It’s important to diversify, whether that’s water treatment, cryogenics, military, or nuclear,” said Harrison. “In North America, we have a huge opportunity to continue developing and staying current with what’s being done in Europe. We continue to invest and develop and find our place on the world stage. We are constantly evolving both from hardware, software, equipment, and people. That's really what it's about.”
About the Author
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
What software automation means for custom fabrication
Why employee-owned companies make sense in manufacturing
Press brakes, panel benders, and flat blank calculations
Nucor’s weekly steel price announcement continues to rattle markets
Educating, rather than just training, tomorrow's workforce
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,